性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | ||
比重 | ASTMD792 | 1.14 | g/cm3 | ||
收缩率-流动 | ASTMD955 | 1.3to1.5 | % | ||
吸水率(平衡,23°C,60%RH) | ASTMD570 | 1.8 | % | ||
ComonomerContent | <0.8 | % | |||
含水量 | <1000 | ppm | |||
相对粘度2 | 2.6to2.7 | ||||
Colorb | -3.80to1.80 | ||||
ColorL | 70.0to78.0 | ||||
抗张强度(23°C) | ASTMD638 | 76.5 | MPa | ||
伸长率(断裂,23°C) | ASTMD638 | 46 | % | ||
弯曲模量(23°C) | ASTMD790 | 2780 | MPa | ||
弯曲强度(23°C) | ASTMD790 | 124 | MPa | ||
悬壁梁缺口冲击强度(23°C) | ASTMD256 | 74 | J/m | ||
载荷下热变形温度(0.45MPa,未退火) | ASTMD648A | 180 | °C | ||
载荷下热变形温度(1.8MPa,未退火) | ASTMD648A | 65.0 | °C | ||
熔融峰值温度 | ASTMD3418 | 220 | °C | ||
线形热膨胀系数-流动 | ASTMD696 | 8.0E-5 | cm/cm/°C | ||
介电强度 | ASTMD149 | 20 | kV/mm | ||
介电常数(1MHz) | ASTMD150 | 3.40 | |||
耐电弧性 | ASTMD495 | 120 | sec | ||
UL阻燃等级 | UL94 | HB | |||
补充信息 | TestMethod | NominalValue | Unit | ||
AminoEndGroups | 42to62 | meq/kg | |||
关于韩国可隆 KOPA® KN181D价格 | |||||
1.有关“PA6 韩国可隆 KOPA® KN181D”物性表及PA6塑胶原料价格以出厂实时数据为准. 2.更多塑胶原料的需求请与我们联系. |
本文链接:http://www.28at.com/showinfo-41-23251-0.htmlPA6 韩国可隆 KOPA® KN181D
声明:本网页内容旨在传播知识,不代表本站观点,若有侵权等问题请及时与本网联系,我们将在第一时间删除处理。