其它 其它 其它 | |
特性:玻纤增强45% |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | ||
成型收缩率 | UBEmethod | 0.4 | % | ||
成型收缩率 | UBEmethod | 1.1 | % | ||
吸水率 | ASTM D-570 | 0.4 | % | ||
吸水率 | ASTM D-570 | 4.8 | % | ||
比重 | ASTM D-792 | 1.50 | |||
抗冲击强度 | 23° | ASTM D-256 | 11 | kgf.cm/cm | |
弯曲强度 | 23° | ASTM D-790 | 2100 | kgf/cm | |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 100 | ||
硬度(洛氏、布氏) | 23° | ASTM D-785 | 115 | ||
屈服下的伸张强度 | 23° | ASTM D-638 | 2200 | kgf/cm | |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 120 | ||
抗冲击强度 | 23° | ASTM D-256 | 15 | kgf.cm/cm | |
弯曲强度 | 23° | ASTM D-790 | 3000 | kgf/cm | |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 95 | ||
断裂下的延伸率 | 23° | ASTM D-638 | 5 | % | |
弯曲弹性率 | 23° | ASTM D-790 | 125000 | kgf/cm | |
屈服下的伸张强度 | 23° | ASTM D-638 | 1700 | kgf/cm | |
弯曲弹性率 | 23° | ASTM D-790 | 89000 | kgf/cm | |
体积电阻率 | ASTM D-257 | 10 | Ω.cm | ||
IEC电路 | UL 746 | 600+ | V | ||
介电损耗 | 10 | ASTM D-150 | 0.01 | ||
体积电阻率 | ASTM D-257 | 10 | Ω.cm | ||
抗电弧强度 | ASTM D-495 | 127 | S | ||
介电损耗 | 10 | ASTM D-150 | 0.01 | ||
介电常数 | 60HZ | ASTM D-150 | 4.3 | ||
介电损耗 | ASTM D-150 | 60HZ | 0.01 | ||
介电常数 | 10 | ASTM D-150 | 3.8 | ||
介电常数 | 10 | ASTM D-150 | 4.2 | ||
热变形温度 | 18.6kgf/cm | ASTM D-648 | 255 | °C | |
熔点 | DSC | 255-265 | °C | ||
燃烧率 | UL 94 | HB | |||
线性热膨胀系数 | ASTM D-696 | 2 | X的10 | ||
关于日本宇部 2020GC9价格 | |||||
1.有关“PA66 日本宇部 2020GC9”物性表及PA66塑料颗粒价格以出厂实时数据为准. 2.更多塑料颗粒的需求请与我们联系. |
本文链接:http://www.28at.com/showinfo-42-26392-0.htmlPA66 日本宇部 2020GC9
声明:本网页内容旨在传播知识,不代表本站观点,若有侵权等问题请及时与本网联系,我们将在第一时间删除处理。