其它 其它 其它 | |
特性:玻璃45%强化,高模敷,高冲击。 |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | ||
吸水率 | 23℃,24小时 | ASTM D-570 | 无水|0.9 | % | |
吸水率 | 23℃,24小时 | ASTM D-570 | 1.9%水|- | % | |
比重 | ASTM D-792 | 无水|1.5 | |||
比重 | ASTM D-792 | 1.9%水|- | |||
泰伯磨耗量 | 1000g,CS-17 | ASTM D-1044 | 无水|30 | mg/1000次 | |
泰伯磨耗量 | 1000g,CS-17 | ASTM D-1044 | 1.9%水|- | mg/1000次 | |
断裂伸长率 | 23℃ | ASTM D-638 | 无水|5 | % | |
断裂伸长率 | 23℃ | ASTM D-638 | 1.9%水|5 | % | |
IZOD冲击强度 | -40℃,无缺口1/8 | ASTM D-256 | 无水|12.5 | kgcm/cm | |
IZOD冲击强度 | -40℃,无缺口1/8 | ASTM D-256 | 1.9%水|15 | kgcm/cm | |
IZOD冲击强度 | -40℃,无缺口1/8 | ASTM D-256 | 无水|12.5 | kgcm/cm2 | |
IZOD冲击强度 | -40℃,无缺口1/8 | ASTM D-256 | 1.9%水|15 | kgcm/cm2 | |
IZOD冲击强度 | 23℃,V缺口1/2 | ASTM D-256 | 无水|15 | kgcm/cm | |
IZOD冲击强度 | 23℃,V缺口1/2 | ASTM D-256 | 1.9%水|20 | kgcm/cm | |
IZOD冲击强度 | 23℃,无缺口1/8 | ASTM D-256 | 无水|98 | kgcm/cm | |
IZOD冲击强度 | 23℃,无缺口1/8 | ASTM D-256 | 1.9%水|120 | kgcm/cm | |
挠曲模量 | 23℃ | ASTM D-790 | 无水|122000 | Kg/cm2 | |
挠曲模量 | 23℃ | ASTM D-790 | 1.9%水|72000 | Kg/cm2 | |
挠曲模量 | 80℃ | ASTM D-790 | 无水|63000 | Kg/cm2 | |
挠曲模量 | 80℃ | ASTM D-790 | 1.9%水|45000 | Kg/cm2 | |
挠曲模量 | -40℃ | ASTM D-790 | 无水|140000 | Kg/cm2 | |
挠曲模量 | -40℃ | ASTM D-790 | 1.9%水|120000 | Kg/cm2 | |
洛氏硬度 | 23℃ | ASTM D-785 | 无水|95 | M-标度 | |
洛氏硬度 | 23℃ | ASTM D-785 | 1.9%水|- | M-标度 | |
洛氏硬度 | 23℃ | ASTM D-785 | 无水|121 | R-标度 | |
洛氏硬度 | 23℃ | ASTM D-785 | 1.9%水|- | R-标度 | |
抗剪强度 | 23℃ | ASTM D-732 | 无水|940 | Kg/cm2 | |
抗剪强度 | 23℃ | ASTM D-732 | 1.9%水|750 | Kg/cm2 | |
挠曲强度 | 23℃ | ASTM D-790 | 无水|2900 | Kg/cm2 | |
挠曲强度 | 23℃ | ASTM D-790 | 1.9%水|1850 | Kg/cm2 | |
挠曲强度 | 80℃ | ASTM D-790 | 无水|16000 | Kg/cm2 | |
挠曲强度 | 80℃ | ASTM D-790 | 1.9%水|- | Kg/cm2 | |
挠曲强度 | -40℃ | ASTM D-790 | 无水|3300 | Kg/cm2 | |
挠曲强度 | -40℃ | ASTM D-790 | 1.9%水|- | Kg/cm2 | |
抗拉屈服强度 | 23℃ | ASTM D-638 | 无水|2000 | Kg/cm2 | |
抗拉屈服强度 | 23℃ | ASTM D-638 | 1.9%水|1300 | Kg/cm2 | |
抗拉屈服强度 | 80℃ | ASTM D-638 | 无水|1200 | Kg/cm2 | |
抗拉屈服强度 | 80℃ | ASTM D-638 | 1.9%水|- | Kg/cm2 | |
抗拉屈服强度 | -40℃ | ASTM D-638 | 无水|2900 | Kg/cm2 | |
抗拉屈服强度 | -40℃ | ASTM D-638 | 1.9%水|- | Kg/cm2 | |
压缩强度 | 23℃ | ASTM D-695 | 无水|1900 | Kg/cm2 | |
压缩强度 | 23℃ | ASTM D-695 | 1.9%水|- | Kg/cm2 | |
压缩强度 | 80℃ | ASTM D-695 | 无水|1000 | Kg/cm2 | |
压缩强度 | 80℃ | ASTM D-695 | 1.9%水|- | Kg/cm2 | |
压缩强度 | -40℃ | ASTM D-695 | 无水|2600 | Kg/cm2 | |
压缩强度 | -40℃ | ASTM D-695 | 1.9%水|- | Kg/cm2 | |
抗电弧性 | 1/8 | ASTM D-495 | 无水|104 | s | |
抗电弧性 | 1/8 | ASTM D-495 | 1.9%水|119 | s | |
介电强度 | 1/8 | ASTM D-149 | 无水|19 | KV/mm | |
介电强度 | 1/8 | ASTM D-149 | 1.9%水|15 | KV/mm | |
介电常数 | 106Hz | ASTM D-150 | 无水|4.2 | ||
介电常数 | 106Hz | ASTM D-150 | 1.9%水|4.5 | ||
介电常数 | 103Hz | ASTM D-150 | 无水|4.9 | ||
介电常数 | 103Hz | ASTM D-150 | 1.9%水|7.4 | ||
体积电阻率 | ASTM D-257 | 无水|1015 | Ω.cm | ||
体积电阻率 | ASTM D-257 | 1.9%水|1012 | Ω.cm | ||
损耗因数 | 50Hz | ASTM D-150 | 无水|0.03 | ||
关于日本东丽 CM1011G-45价格 | |||||
1.有关“PA66 日本东丽 CM1011G-45”物性表及PA66塑胶原料价格以出厂实时数据为准. 2.更多塑胶原料的需求请与我们联系. |
本文链接:http://www.28at.com/showinfo-42-26334-0.htmlPA66 日本东丽 CM1011G-45